1018 steel heat treatment
The everyday mild steel. Too low in carbon to through-harden; case-harden it or use it as machined. Typical practice for AISI 1018: carburize at 900 to 925 °C (1650 to 1695 °F), quench (oil or water after carburizing), then temper at 150 to 200 °C (300 to 390 °F).
- Carburize
- 900 to 925 °C
- 1650 to 1695 °F
- Temper
- 150 to 200 °C
- 300 to 390 °F
- Quench
- Oil or water after carburizing
- Typical hardness
- Case about 58 to 62 HRC, core stays soft
Not a through-hardening steel. Gas or pack carburize to build a high-carbon case, quench, then temper low. As-supplied cold-drawn bar is often used with no heat treatment at all.
Typical published practice for guidance. Section size, prior condition, furnace accuracy and soak time all shift the right numbers. Verify against your steel supplier's datasheet before hardening anything that matters.
1018 chemical composition
| Element | Symbol | Weight % |
|---|---|---|
| Carbon | C | 0.15 to 0.2 |
| Manganese | Mn | 0.6 to 0.9 |
These are the limits of the standard's chemical range. Low-carbon steel. Also known as: C15 (near), S15C (near), En3 (near).
1018 critical temperatures
| Temperature | What it means | Estimate | Equation |
|---|---|---|---|
| Ac1 | Lower critical temperature | about 715 °C (1319 °F) | Ac1 = 723 - 10.7 Mn - 16.9 Ni + 29.1 Si + 16.9 Cr + 6.38 W |
| Ac3 | Upper critical temperature | about 825 °C (1517 °F) | Ac3 = 910 - 203 sqrt(C) + 44.7 Si - 15.2 Ni + 31.5 Mo + 104 V + 13.1 W |
| Ms | Martensite start | about 442 °C (828 °F) | Ms = 539 - 423 C - 30.4 Mn - 17.7 Ni - 12.1 Cr - 7.5 Mo |
Estimates from the mid-range composition, with element amounts in weight per cent. Correlations like these scatter by about 20 to 25 °C against measurement, and real values shift with heating rate. Source: K.W. Andrews, "Empirical formulae for the calculation of some transformation temperatures", Journal of the Iron and Steel Institute, 203 (1965) 721-727.
Questions
- What temperature do you carburize 1018 steel at?
- Carburize 1018 at 900 to 925 °C (1650 to 1695 °F), then quench: oil or water after carburizing. This is typical published practice; section size and furnace accuracy shift the right number.
- What temperature do you temper 1018 at?
- Temper 1018 at 150 to 200 °C (300 to 390 °F). Typical hardness: case about 58 to 62 HRC, core stays soft.
- What do you quench 1018 steel in?
- Oil or water after carburizing. Not a through-hardening steel. Gas or pack carburize to build a high-carbon case, quench, then temper low. As-supplied cold-drawn bar is often used with no heat treatment at all.
- What is 1018 steel equivalent to?
- Other designations for 1018, or for its nearest equivalent where marked "near": C15 (near), S15C (near), En3 (near). Check the chemistry on your supplier's datasheet before treating them as the same steel.
Other carbon steels
- 1045Medium-carbon steel
- 1060Medium-high carbon steel
- 1075High-carbon steel
- 1080High-carbon steel
- 1084High-carbon steel
- 1095High-carbon steel
- 15N20Nickel band steel
- 26C3Very high carbon steel
Sources for this grade: SAE J403 chemical ranges; Typical published practice.
Enter your own composition and get the numbers, with sources.
Heat treatment numbers for common steels, each traced to its source paper. About HeatTreat