26C3 steel heat treatment
Very high purity, very high carbon razor steel. Extremely keen edges and vivid hamons in skilled hands. Typical practice for 26C3: austenitize at 790 to 815 °C (1455 to 1500 °F), quench (fast oil, brine only on thin blades by experienced hands), then temper at 150 to 200 °C (300 to 390 °F).
- Austenitize
- 790 to 815 °C
- 1455 to 1500 °F
- Temper
- 150 to 200 °C
- 300 to 390 °F
- Quench
- Fast oil, brine only on thin blades by experienced hands
- Typical hardness
- 62 to 65 HRC after a low temper
Keep soaks short and temperatures low so the large carbon reserve stays mostly in carbide. Shallow hardening: thick spines stay soft and hamons come easily.
Typical published practice for guidance. Section size, prior condition, furnace accuracy and soak time all shift the right numbers. Verify against your steel supplier's datasheet before hardening anything that matters.
26C3 chemical composition
| Element | Symbol | Weight % |
|---|---|---|
| Carbon | C | 1.25 |
| Manganese | Mn | 0.35 |
| Silicon | Si | 0.25 |
These are the producer's typical values, not a standard range. Very high carbon steel. Also known as: 1.1282 (near).
26C3 critical temperatures
| Temperature | What it means | Estimate | Equation |
|---|---|---|---|
| Ac1 | Lower critical temperature | Withheld | Ac1 = 723 - 10.7 Mn - 16.9 Ni + 29.1 Si + 16.9 Cr + 6.38 W |
| Ac3 | Upper critical temperature | Withheld | Ac3 = 910 - 203 sqrt(C) + 44.7 Si - 15.2 Ni + 31.5 Mo + 104 V + 13.1 W |
| Ms | Martensite start | Withheld | Ms = 539 - 423 C - 30.4 Mn - 17.7 Ni - 12.1 Cr - 7.5 Mo |
Carbon near 1.25% is beyond the range these correlations were fitted to.
Estimates from the mid-range composition, with element amounts in weight per cent. Correlations like these scatter by about 20 to 25 °C against measurement, and real values shift with heating rate. Source: K.W. Andrews, "Empirical formulae for the calculation of some transformation temperatures", Journal of the Iron and Steel Institute, 203 (1965) 721-727.
Questions
- What temperature do you harden 26C3 steel at?
- Austenitize 26C3 at 790 to 815 °C (1455 to 1500 °F), then quench: fast oil, brine only on thin blades by experienced hands. This is typical published practice; section size and furnace accuracy shift the right number.
- What temperature do you temper 26C3 at?
- Temper 26C3 at 150 to 200 °C (300 to 390 °F). Typical hardness: 62 to 65 HRC after a low temper.
- What do you quench 26C3 steel in?
- Fast oil, brine only on thin blades by experienced hands. Keep soaks short and temperatures low so the large carbon reserve stays mostly in carbide. Shallow hardening: thick spines stay soft and hamons come easily.
- What is 26C3 steel equivalent to?
- Other designations for 26C3, or for its nearest equivalent where marked "near": 1.1282 (near). Check the chemistry on your supplier's datasheet before treating them as the same steel.
Other carbon steels
- 1018Low-carbon steel
- 1045Medium-carbon steel
- 1060Medium-high carbon steel
- 1075High-carbon steel
- 1080High-carbon steel
- 1084High-carbon steel
- 1095High-carbon steel
- 15N20Nickel band steel
Sources for this grade: Producer datasheets (typical values); Typical published practice.
Enter your own composition and get the numbers, with sources.