1075 vs 1084 steel

1075 (High-carbon steel). Forgiving high-carbon steel for blades and springs, a small step milder than 1080.

1084 (High-carbon steel). The classic beginner blade steel: eutectoid carbon, wide forgiving windows, clean results in a home shop.

How 1075 and 1084 differ

  • 1084 carries more carbon: 0.8 to 0.93% against 0.7 to 0.8% in 1075.
  • Both are austenitized in much the same range: 800 to 830 °C for 1075 and 800 to 830 °C for 1084.
  • Both are quenched the same way: fast oil.

Side by side

1075 and 1084 compared
10751084
TypeHigh-carbon steelHigh-carbon steel
Carbon (C), wt %0.7 to 0.80.8 to 0.93
Manganese (Mn), wt %0.4 to 0.70.6 to 0.9
Austenitize800 to 830 °C (1470 to 1525 °F)800 to 830 °C (1470 to 1525 °F)
QuenchFast oilFast oil
Temper175 to 260 °C (345 to 500 °F)175 to 230 °C (345 to 445 °F)
Typical hardness55 to 58 HRC after a 200 C temper57 to 60 HRC after a 190 to 200 C temper
Ac1 (lower critical temperature)about 717 °C (1323 °F)about 715 °C (1319 °F)
Ac3 (upper critical temperature)about 734 °C (1354 °F)Withheld
Ms (martensite start)about 205 °C (401 °F)about 150 °C (303 °F)

Ac1, Ac3 and Ms are estimates from the Andrews (1965) correlations at mid-range composition. They are withheld where a steel falls outside the low-alloy range those correlations cover, and Ac3 is withheld for steels above about 0.8% carbon. Typical published practice for guidance. Section size, prior condition, furnace accuracy and soak time all shift the right numbers. Verify against your steel supplier's datasheet before hardening anything that matters.

Heat treating each one

1075

Lower manganese than 1080 makes it slightly shallower hardening. A good hamon candidate in thin sections with a fast quench.

1084

At eutectoid carbon everything transforms cleanly with no excess carbide to manage. Normalize after forging, then harden from a low soak. Pattern-welds beautifully against 15N20.

Questions

What is the difference between 1075 and 1084 steel?
1084 carries more carbon: 0.8 to 0.93% against 0.7 to 0.8% in 1075. Both are austenitized in much the same range: 800 to 830 °C for 1075 and 800 to 830 °C for 1084.
Is 1075 or 1084 harder after heat treatment?
Typical hardness for 1075: 55 to 58 HRC after a 200 C temper. For 1084: 57 to 60 HRC after a 190 to 200 C temper. The result depends on the temper you choose.
Can I heat treat 1075 and 1084 the same way?
No, each has its own recipe. 1075: austenitize at 800 to 830 °C, quench in fast oil, temper at 175 to 260 °C. 1084: austenitize at 800 to 830 °C, quench in fast oil, temper at 175 to 230 °C.

Heat treatment numbers for your own steel, with sources.