420 steel heat treatment
The entry martensitic stainless: scalpels, scissors and budget blades. Modest hardness, easy care. Typical practice for 420: austenitize at 980 to 1035 °C (1795 to 1895 °F), quench (air or oil), then temper at 150 to 370 °C (300 to 700 °F).
- Austenitize
- 980 to 1035 °C
- 1795 to 1895 °F
- Temper
- 150 to 370 °C
- 300 to 700 °F
- Quench
- Air or oil
- Typical hardness
- 48 to 53 HRC
The specification sets carbon as a 0.15 minimum; cutlery heats run higher within the range shown. Avoid tempering between about 425 and 600 C, which sacrifices both corrosion resistance and toughness.
Typical published practice for guidance. Section size, prior condition, furnace accuracy and soak time all shift the right numbers. Verify against your steel supplier's datasheet before hardening anything that matters.
420 chemical composition
| Element | Symbol | Weight % |
|---|---|---|
| Carbon | C | 0.15 to 0.4 |
| Manganese | Mn | 1 max |
| Silicon | Si | 1 max |
| Chromium | Cr | 12 to 14 |
These are the limits of the standard's chemical range. Martensitic stainless steel. Also known as: 1.4021, X20Cr13, SUS420J1.
420 critical temperatures
| Temperature | What it means | Estimate | Equation |
|---|---|---|---|
| Ac1 | Lower critical temperature | Withheld | Ac1 = 723 - 10.7 Mn - 16.9 Ni + 29.1 Si + 16.9 Cr + 6.38 W |
| Ac3 | Upper critical temperature | Withheld | Ac3 = 910 - 203 sqrt(C) + 44.7 Si - 15.2 Ni + 31.5 Mo + 104 V + 13.1 W |
| Ms | Martensite start | Withheld | Ms = 539 - 423 C - 30.4 Mn - 17.7 Ni - 12.1 Cr - 7.5 Mo |
Chromium near 13.0% puts 420 outside the low-alloy steels these correlations were fitted to. High-chromium tool and stainless steels need measured data.
Estimates from the mid-range composition, with element amounts in weight per cent. Correlations like these scatter by about 20 to 25 °C against measurement, and real values shift with heating rate. Source: K.W. Andrews, "Empirical formulae for the calculation of some transformation temperatures", Journal of the Iron and Steel Institute, 203 (1965) 721-727.
Questions
- What temperature do you harden 420 steel at?
- Austenitize 420 at 980 to 1035 °C (1795 to 1895 °F), then quench: air or oil. This is typical published practice; section size and furnace accuracy shift the right number.
- What temperature do you temper 420 at?
- Temper 420 at 150 to 370 °C (300 to 700 °F). Typical hardness: 48 to 53 HRC.
- What do you quench 420 steel in?
- Air or oil. The specification sets carbon as a 0.15 minimum; cutlery heats run higher within the range shown. Avoid tempering between about 425 and 600 C, which sacrifices both corrosion resistance and toughness.
- What is 420 steel equivalent to?
- Other designations for 420, or for its nearest equivalent where marked "near": 1.4021, X20Cr13, SUS420J1. Check the chemistry on your supplier's datasheet before treating them as the same steel.
Other stainless steels
- 440CMartensitic stainless steel
- AEB-LMartensitic stainless steel
- 154CMMartensitic stainless steel
- MagnaCutPowder-metallurgy stainless steel
Sources for this grade: ASTM A276 (C specified as a minimum); Typical published practice.