420 vs 440C steel

420 (Martensitic stainless steel). The entry martensitic stainless: scalpels, scissors and budget blades. Modest hardness, easy care.

440C (Martensitic stainless steel). The classic high-hardness stainless for bearings, valve seats and knives that must not rust.

How 420 and 440C differ

  • 440C carries more carbon: 0.95 to 1.2% against 0.15 to 0.4% in 420.
  • 440C is alloyed with molybdenum (0.75 max%), which 420 does not have in any real amount.
  • 440C has far more chromium: 16 to 18% against 12 to 14%.
  • 440C is austenitized hotter: 1010 to 1065 °C (1850 to 1950 °F) against 980 to 1035 °C (1795 to 1895 °F) for 420.
  • The quench differs. 420: air or oil. 440C: air, plates, or oil.

Side by side

420 and 440C compared
420440C
TypeMartensitic stainless steelMartensitic stainless steel
Carbon (C), wt %0.15 to 0.40.95 to 1.2
Manganese (Mn), wt %1 max1 max
Silicon (Si), wt %1 max1 max
Chromium (Cr), wt %12 to 1416 to 18
Molybdenum (Mo), wt %none listed0.75 max
Austenitize980 to 1035 °C (1795 to 1895 °F)1010 to 1065 °C (1850 to 1950 °F)
QuenchAir or oilAir, plates, or oil
Temper150 to 370 °C (300 to 700 °F)150 to 230 °C (300 to 445 °F)
Typical hardness48 to 53 HRC57 to 60 HRC
Ac1 (lower critical temperature)WithheldWithheld
Ac3 (upper critical temperature)WithheldWithheld
Ms (martensite start)WithheldWithheld

Ac1, Ac3 and Ms are estimates from the Andrews (1965) correlations at mid-range composition. They are withheld where a steel falls outside the low-alloy range those correlations cover, and Ac3 is withheld for steels above about 0.8% carbon. Typical published practice for guidance. Section size, prior condition, furnace accuracy and soak time all shift the right numbers. Verify against your steel supplier's datasheet before hardening anything that matters.

Heat treating each one

420

The specification sets carbon as a 0.15 minimum; cutlery heats run higher within the range shown. Avoid tempering between about 425 and 600 C, which sacrifices both corrosion resistance and toughness.

440C

Cold treatment after the quench is common to convert retained austenite. Avoid tempering between about 425 and 565 C, where corrosion resistance and toughness both fall.

Questions

What is the difference between 420 and 440C steel?
440C carries more carbon: 0.95 to 1.2% against 0.15 to 0.4% in 420. 440C is alloyed with molybdenum (0.75 max%), which 420 does not have in any real amount.
Is 420 or 440C harder after heat treatment?
Typical hardness for 420: 48 to 53 HRC. For 440C: 57 to 60 HRC. The result depends on the temper you choose.
Can I heat treat 420 and 440C the same way?
No, each has its own recipe. 420: austenitize at 980 to 1035 °C, quench in air or oil, temper at 150 to 370 °C. 440C: austenitize at 1010 to 1065 °C, quench in air, plates, or oil, temper at 150 to 230 °C.

Heat treatment numbers for your own steel, with sources.

Heat treatment numbers for common steels, each traced to its source paper. About HeatTreat